In the field of electrochemistry, platinum is used as an anode material, which has excellent performance. Especially in the process of electrochemical anodic oxygen evolution in an acidic medium, platinum has no oxidation resistance and electrocatalysis performance that other materials have. Platinum is used as an anode material in many important electrochemical production fields, such as hydrogen peroxide, ammonium persulfate, etc. However, platinum resources are scarce and expensive. In order to reduce costs and maintain the excellent performance of platinum anodes, platinum-plated anode materials have been studied to replace pure platinum electrode products, and good results have been achieved.
Anodul de titan placat cu platină este un proces de placare cu platină pe bază de titan. Un strat de acoperire cu platină pură este depus pe suprafața de titan. Fluxul de proces al anodului de titan placat cu platină este următorul:
Pretratarea foii de titan → curățare electro → spălare cu apă → activare → spălare cu apă distilată → placare cu perie platină → spălare cu apă distilată → uscare

Specificațiile de bază sunt următoarele:
Material de bază: titan (Gr1, Gr2, TA1, TA2)
Formă: reticulat, tabular, tubular sau personalizat în funcție de cerințele clientului
Densitatea curentului: < 8000 A/m2
Proces de fabricație: galvanizare
Material de acoperire: platină (puritate 99,99%)
Conținut de metale prețioase: mai mare sau egal cu 21,48 g/㎡
Grosimea stratului de platină: 0.3-15 μ m
Temperatura: < 80 de grade
Valoarea PH: 1-12